HK40 Creep Resistant High Temp Cast Grate Bars For Waste Incineration Boiler
HK40 high-temperature alloy cast grate bars feature outstanding high-temperature creep resistance, oxidation resistance and thermal fatigue performance, customized as core bearing and combustion parts for municipal solid waste, industrial waste and hazardous waste incineration boilers under long-term ultra-high temperature and alternating thermal load.
| C | Cr | Ni | Si | Mn | S | P |
|---|---|---|---|---|---|---|
| 0.35–0.45 | 23.0–27.0 | 18.0–22.0 | ≤2.0 | ≤2.0 | ≤0.05 | ≤0.05 |
- Continuous service temperature: 900–1100℃
- Stable austenitic microstructure at high temperature, effectively inhibit high-temperature creep deformation
- Excellent anti-oxidation performance, slow surface scaling under long-term waste incineration flue gas erosion
- Strong thermal shock resistance, no cracking under frequent furnace charging and cooling cycles
- Good corrosion resistance against sulfur, chlorine flue gas generated from waste combustion
- High chromium-nickel HK40 alloy formula greatly restricts permanent creep deformation under long-term high-temperature bearing load, effectively avoid grate bar bending and jamming
- Optimized grate tooth and ventilation slot structure, improve combustion efficiency while reducing ash abrasion on the base body
- Complete homogenization heat treatment eliminates casting internal stress, prevent thermal fatigue crack failure during long-term incineration operation
- Strong resistance to chlorine and sulfur corrosive flue gas unique to waste incineration, outperforms ordinary low-alloy heat-resistant castings
- Customizable single-piece length, tooth spacing and support structure according to boiler incineration capacity and waste calorific value
Mobile grate bars, stationary grate bars, side sealing grate blocks, connecting castings, ash baffle plates all made of HK40 alloy
A: Waste incineration brings sustained high temperature, sulfur/chlorine corrosive flue gas and frequent thermal cycles. HK40 has top-tier creep resistance to prevent bending deformation, and resists oxidation & flue gas corrosion, solving the frequent replacement problem of ordinary grate bars.
A: Yes, we adjust ventilation gaps, tooth thickness and overall structural strength targeting domestic garbage, industrial hazardous waste and biomass waste.
A: Full inspection documents including creep performance, thermal shock, metallographic and NDT reports can be supplied for power plant project acceptance.
- Dedicated HK40 high-nickel alloy smelting and homogenization heat treatment production line
- Rich manufacturing experience supporting waste incineration power plant boiler spare parts
- Strict raw material composition control to stabilize high-temperature creep resistance
- Stable mass supply for global solid waste incineration and thermal energy recovery projects