MOQ: | 30 kg |
Price: | USD80/kg ~ USD120/kg |
Standard Packaging: | Pallets |
Delivery Period: | It depends on the quantity to be ordered. |
Payment Method: | by T/T or L/C |
Supply Capacity: | 100,000,000.00 |
We produce High Temperature Superalloy Castings Parts with centrifugal cast process, wax cast process and resin sand cast process.
Our alloys can be cut using any conventional plasma arc cutting system. The best arc quality is achieved using a mixture of argon and hydrogen gases. Nitrogen gas can be substituted for hydrogen gases, but the cut quality will deteriorate slightly. Shop air or any oxygen bearing gases should be avoided when plasma cutting these alloys.
Table 1 : Standard Cobalt cobalt alloy Alloy
Co | Cr | C | W | Mo | Ni | Si | B | Fe | Mn | Others | |
cobalt alloy 1 | BAL | 33 | 2.45 | 13 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 3 | BAL | 31 | 2.5 | 13 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 4 | BAL | 31.5 | 1 | 14 | - | 2.0* | 1 | - | 2.0* | 1 | - |
BAL | 28 | 1.2 | 5 | - | 3.0* | 1 | - | 2.5* | 1 | - | |
cobalt alloy 12 | BAL | 29 | 1.85 | 9 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 20 | BAL | 33 | 2.45 | 17.5 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 21 | BAL | 27 | 0.25 | - | 5.5 | 2.5* | 1 | - | 3.0* | 1 | - |
cobalt alloy 31 | BAL | 26 | 0.5 | 7.5 | - | 10.5 | 1 | - | 2.0* | 1 | - |
cobalt alloy 190 | BAL | 26 | 3.3 | 14 | - | 1.0 | 1 | - | 8.0 | 0.5 | - |
cobalt alloy 238 | BAL | 26 | 0.1 | - | 3 | - | 1 | - | 20.0 | 1 | - |
cobalt alloy 306 | BAL | 25 | 0.4 | 2 | - | 6.0 | 1 | - | 4.0* | 1 | Nb=5 |
94 | BAL | 28 | 1 | 19 | - | 5.0 | 1 | - | 2.5* | 1 | V=1 |
cobalt alloy F | BAL | 25.5 | 1.75 | 12.25 | - | 22.5 | 1 | - | 1.5* | - | - |
cobalt alloy SF1 | BAL | 19 | 1.3 | 13 | - | 13 | 3 | 2.5 | 3* | 0.5 | Cu=0.5 |
cobalt alloy SF6 | BAL | 19 | 0.7 | 7 | - | 13 | 2.5 | 1.7 | 3* | 0.5 | Cu=0.5 |
cobalt alloy SF12 | BAL | 19 | 1 | 9 | - | 13 | 3 | 2 | 3* | 0.5 | Cu=0.5 |
cobalt alloy SF20 | BAL | 19 | 1.5 | 15 | - | 13 | 3 | 3 | 2* | 0.5 | Cu=0.5 |
TRIBALOY T400 | BAL | 8 | 0.1* | - | 28 | 3* | 2.4 | - | 3* | - | - |
TRIBALOY T800 | BAL | 17 | 0.1* | - | 28 | 3* | 3.2 | - | 3* | - | - |
DELORO 15 | - | - | 0.06* | - | - | BAL | 2.0 | 1.05 | 1.5* | 20 | Cu=20 |
DELORO 22 | - | 0.70 | 0.10 | - | - | BAL | 2.3 | 1.75 | - | - | - |
DELORO 40 | - | 7.0 | 0.10 | - | - | BAL | 3.5 | 2.25 | - | - | - |
DELORO 50 | - | 10.25 | 0.45 | - | - | BAL | 4.0 | 1.85 | 4.0 | - | - |
DELORO 60 | - | 14.25 | 0.6 | - | - | BAL | 2.0 | 3.5 | 4.0 | - | - |
DELORO 625 | - | 22 | 0.1 | - | 9 | BAL | - | - | 5 | - | - |
NISTELLE C | - | 16.5 | 0.12* | 4.5 | 17 | BAL | 0.7 | - | 6.0 | - | - |
TRIBALOY T700 | - | 15 | 0.10* | - | 32 | BAL | 3.25 | - |
Hastelloy C22®(UNS N06022)(Max.) | ||||||||||||
C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | V | |
0.015 | 0.5 | 0.02 | 0.02 | 0.08 | 20.0-22.5 | Bal. | 12.5-14.5 | 2.5 | 2.0-6.0 | 2.5-3.5 | 0.35 | |
Hastelloy C276®(UNS N10276)(Max.) | ||||||||||||
C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | V | |
0.01 | 1 | 0.04 | 0.03 | 0.08 | 14.5-16.5 | Bal. | 15.0-17.0 | 2.5 | 4.0-7.0 | 3.0-4.5 | 0.35 | |
Hastelloyx®(UNS N06002)(Max.) | ||||||||||||
C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | other | |
0.05-0.15 | 1 | 0.04 | 0.03 | 1 | 20.5-23.0 | Bal. | 8.0-10.0 | 0.5-2.5 | 17.0-20.0 | 0.2-1.0 | / | |
Monel 400®(UNS NO4400) (Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Fe | ||||||
0.3 | 2 | 0.024 | 0.5 | 63 min | 28-34 | 2.5 | ||||||
Monel M400®(UNS NO4400)(Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Fe | ||||||
0.3 | 2 | 0.024 | 0.5 | 63-70 | 28-34 | 2.5 | ||||||
Monel R405®(UNS NO4405)(Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Fe | ||||||
0.3 | 2 | 0.025-0.06 | 0.5 | 63.0min | 28-34 | 2.5 | ||||||
Monel K500®(UNS NO5500)(Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Ti | AI | Fe | ||||
0.1 | 2 | 0.01 | 0.5 | 63min | 27-33 | 0.86 | 2.3-3.15 | 2 | ||||
Inconel 600(UNS NO6600)(Max.) | ||||||||||||
C | MN | S | Si | Cr | Ni | Cu | Fe | |||||
0.15 | 1 | 0.015 | 0.5 | 14-17 | 72 min | 0.5 | 6.0-10.0 | |||||
Inconel 601(UNS NO6601)(Max.) | ||||||||||||
C | MN | Si | Cr | Ni | CO | AI | Fe | |||||
0.05 | 0.3 | 0.2 | 22.5 | 61.5min | 5 | 1.4 | 14.1 | |||||
Inconel 718(UNS NO7718)(Max.) | ||||||||||||
Cr | Ni | Mo | CO | Cb+Ta | Ti | AI | Fe | |||||
19 | 52.5min | 3.05 | 5 | 5.13 | 0.9 | 0.5 | 18.5 | |||||
Chemical Analysis of Incoloy 800® uns(N08800) | ||||||||||||
C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
0.1 max | 19.0-23.0 | 30.0-35.0 | 0.15-0.6 | 0.15-0.6 | 39.5min | / | ||||||
Incoloy800H® UNS(N08810) | ||||||||||||
C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
0.05-0.1 | 19.0-23.0 | 30.0-35.0 | 0.15-0.60 | 0.15-0.60 | 39.5min | 5or coarser | ||||||
Incoloy800HT® UNS(N08811) | ||||||||||||
C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
0.06-0.10 | 19.0-23.0 | 30.0-35.0 | 0.25-0.60 | 0.25-0.60 | 39.5min | 5or coarser | ||||||
Dimensions:as per drawings
|
Step 1: Getting orders.
Step 2: Process design by technical department
Step 3: Purchase of raw materials and pattern making &checking
Step 4: Inspection of raw materials
Step 5: Melting by middle-frequency induction furnaces
Step 6: Ladle analysis by Spectrometer
Step 7: De-oxidization, slag-removal, tapping
Step 8: Pouring
Step 9: Openning & fettling
Step 10: Surface & dimensional check
Step 11: Heat treatment
Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)
Step 13: Packing
Step 14: Shipping
1. 16-year Foundry Operation Experience.
2. Friendly & High Efficient Technical & Commercial Communication.
3. Professional Export Practices: Have Exported to +60 Overseas Countries.
Our Trade Show
Our booth No. 14-A29-5 in Newcast 2015,Germany
Hall 14, Stand No.A29-5.
MOQ: | 30 kg |
Price: | USD80/kg ~ USD120/kg |
Standard Packaging: | Pallets |
Delivery Period: | It depends on the quantity to be ordered. |
Payment Method: | by T/T or L/C |
Supply Capacity: | 100,000,000.00 |
We produce High Temperature Superalloy Castings Parts with centrifugal cast process, wax cast process and resin sand cast process.
Our alloys can be cut using any conventional plasma arc cutting system. The best arc quality is achieved using a mixture of argon and hydrogen gases. Nitrogen gas can be substituted for hydrogen gases, but the cut quality will deteriorate slightly. Shop air or any oxygen bearing gases should be avoided when plasma cutting these alloys.
Table 1 : Standard Cobalt cobalt alloy Alloy
Co | Cr | C | W | Mo | Ni | Si | B | Fe | Mn | Others | |
cobalt alloy 1 | BAL | 33 | 2.45 | 13 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 3 | BAL | 31 | 2.5 | 13 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 4 | BAL | 31.5 | 1 | 14 | - | 2.0* | 1 | - | 2.0* | 1 | - |
BAL | 28 | 1.2 | 5 | - | 3.0* | 1 | - | 2.5* | 1 | - | |
cobalt alloy 12 | BAL | 29 | 1.85 | 9 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 20 | BAL | 33 | 2.45 | 17.5 | - | 2.5* | 1 | - | 2.5* | 1 | - |
cobalt alloy 21 | BAL | 27 | 0.25 | - | 5.5 | 2.5* | 1 | - | 3.0* | 1 | - |
cobalt alloy 31 | BAL | 26 | 0.5 | 7.5 | - | 10.5 | 1 | - | 2.0* | 1 | - |
cobalt alloy 190 | BAL | 26 | 3.3 | 14 | - | 1.0 | 1 | - | 8.0 | 0.5 | - |
cobalt alloy 238 | BAL | 26 | 0.1 | - | 3 | - | 1 | - | 20.0 | 1 | - |
cobalt alloy 306 | BAL | 25 | 0.4 | 2 | - | 6.0 | 1 | - | 4.0* | 1 | Nb=5 |
94 | BAL | 28 | 1 | 19 | - | 5.0 | 1 | - | 2.5* | 1 | V=1 |
cobalt alloy F | BAL | 25.5 | 1.75 | 12.25 | - | 22.5 | 1 | - | 1.5* | - | - |
cobalt alloy SF1 | BAL | 19 | 1.3 | 13 | - | 13 | 3 | 2.5 | 3* | 0.5 | Cu=0.5 |
cobalt alloy SF6 | BAL | 19 | 0.7 | 7 | - | 13 | 2.5 | 1.7 | 3* | 0.5 | Cu=0.5 |
cobalt alloy SF12 | BAL | 19 | 1 | 9 | - | 13 | 3 | 2 | 3* | 0.5 | Cu=0.5 |
cobalt alloy SF20 | BAL | 19 | 1.5 | 15 | - | 13 | 3 | 3 | 2* | 0.5 | Cu=0.5 |
TRIBALOY T400 | BAL | 8 | 0.1* | - | 28 | 3* | 2.4 | - | 3* | - | - |
TRIBALOY T800 | BAL | 17 | 0.1* | - | 28 | 3* | 3.2 | - | 3* | - | - |
DELORO 15 | - | - | 0.06* | - | - | BAL | 2.0 | 1.05 | 1.5* | 20 | Cu=20 |
DELORO 22 | - | 0.70 | 0.10 | - | - | BAL | 2.3 | 1.75 | - | - | - |
DELORO 40 | - | 7.0 | 0.10 | - | - | BAL | 3.5 | 2.25 | - | - | - |
DELORO 50 | - | 10.25 | 0.45 | - | - | BAL | 4.0 | 1.85 | 4.0 | - | - |
DELORO 60 | - | 14.25 | 0.6 | - | - | BAL | 2.0 | 3.5 | 4.0 | - | - |
DELORO 625 | - | 22 | 0.1 | - | 9 | BAL | - | - | 5 | - | - |
NISTELLE C | - | 16.5 | 0.12* | 4.5 | 17 | BAL | 0.7 | - | 6.0 | - | - |
TRIBALOY T700 | - | 15 | 0.10* | - | 32 | BAL | 3.25 | - |
Hastelloy C22®(UNS N06022)(Max.) | ||||||||||||
C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | V | |
0.015 | 0.5 | 0.02 | 0.02 | 0.08 | 20.0-22.5 | Bal. | 12.5-14.5 | 2.5 | 2.0-6.0 | 2.5-3.5 | 0.35 | |
Hastelloy C276®(UNS N10276)(Max.) | ||||||||||||
C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | V | |
0.01 | 1 | 0.04 | 0.03 | 0.08 | 14.5-16.5 | Bal. | 15.0-17.0 | 2.5 | 4.0-7.0 | 3.0-4.5 | 0.35 | |
Hastelloyx®(UNS N06002)(Max.) | ||||||||||||
C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | other | |
0.05-0.15 | 1 | 0.04 | 0.03 | 1 | 20.5-23.0 | Bal. | 8.0-10.0 | 0.5-2.5 | 17.0-20.0 | 0.2-1.0 | / | |
Monel 400®(UNS NO4400) (Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Fe | ||||||
0.3 | 2 | 0.024 | 0.5 | 63 min | 28-34 | 2.5 | ||||||
Monel M400®(UNS NO4400)(Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Fe | ||||||
0.3 | 2 | 0.024 | 0.5 | 63-70 | 28-34 | 2.5 | ||||||
Monel R405®(UNS NO4405)(Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Fe | ||||||
0.3 | 2 | 0.025-0.06 | 0.5 | 63.0min | 28-34 | 2.5 | ||||||
Monel K500®(UNS NO5500)(Max.) | ||||||||||||
C | MN | S | Si | Ni | Cu | Ti | AI | Fe | ||||
0.1 | 2 | 0.01 | 0.5 | 63min | 27-33 | 0.86 | 2.3-3.15 | 2 | ||||
Inconel 600(UNS NO6600)(Max.) | ||||||||||||
C | MN | S | Si | Cr | Ni | Cu | Fe | |||||
0.15 | 1 | 0.015 | 0.5 | 14-17 | 72 min | 0.5 | 6.0-10.0 | |||||
Inconel 601(UNS NO6601)(Max.) | ||||||||||||
C | MN | Si | Cr | Ni | CO | AI | Fe | |||||
0.05 | 0.3 | 0.2 | 22.5 | 61.5min | 5 | 1.4 | 14.1 | |||||
Inconel 718(UNS NO7718)(Max.) | ||||||||||||
Cr | Ni | Mo | CO | Cb+Ta | Ti | AI | Fe | |||||
19 | 52.5min | 3.05 | 5 | 5.13 | 0.9 | 0.5 | 18.5 | |||||
Chemical Analysis of Incoloy 800® uns(N08800) | ||||||||||||
C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
0.1 max | 19.0-23.0 | 30.0-35.0 | 0.15-0.6 | 0.15-0.6 | 39.5min | / | ||||||
Incoloy800H® UNS(N08810) | ||||||||||||
C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
0.05-0.1 | 19.0-23.0 | 30.0-35.0 | 0.15-0.60 | 0.15-0.60 | 39.5min | 5or coarser | ||||||
Incoloy800HT® UNS(N08811) | ||||||||||||
C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
0.06-0.10 | 19.0-23.0 | 30.0-35.0 | 0.25-0.60 | 0.25-0.60 | 39.5min | 5or coarser | ||||||
Dimensions:as per drawings
|
Step 1: Getting orders.
Step 2: Process design by technical department
Step 3: Purchase of raw materials and pattern making &checking
Step 4: Inspection of raw materials
Step 5: Melting by middle-frequency induction furnaces
Step 6: Ladle analysis by Spectrometer
Step 7: De-oxidization, slag-removal, tapping
Step 8: Pouring
Step 9: Openning & fettling
Step 10: Surface & dimensional check
Step 11: Heat treatment
Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)
Step 13: Packing
Step 14: Shipping
1. 16-year Foundry Operation Experience.
2. Friendly & High Efficient Technical & Commercial Communication.
3. Professional Export Practices: Have Exported to +60 Overseas Countries.
Our Trade Show
Our booth No. 14-A29-5 in Newcast 2015,Germany
Hall 14, Stand No.A29-5.