Send Message
products
PRODUCTS DETAILS
Home > Products >
cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054

cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054

MOQ: 30 kg
Price: USD80/kg ~ USD120/kg
Standard Packaging: Pallets
Delivery Period: It depends on the quantity to be ordered.
Payment Method: by T/T or L/C, Western Union
Supply Capacity: 100,000,000.00
Detail Information
Place of Origin
China
Brand Name
Eternal Bliss
Certification
ISO9001-2008
Model Number
EB26054
Hardness:
More Than HRC 43
Material:
Cobalt Alloy 7
Working Temperature:
Up To 1300 Degree
Corrosion Resistance:
High
Size Tolerance After Casting:
CT7
Certification:
ISO9001
Highlight:

precision steel casting

,

cobalt based alloys

Product Description

cobalt alloy 7 Cobalt Castings High Temperature Up to 1300 Degree Wax Cast Process EB26054

cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 0

We produce High Temperature Superalloy Castings Parts with centrifugal cast process, investment process and resin sand cast process.

 

Cobalt base alloys have been used extensively in the past for high temperature applications and have been found to be generally satisfactory except that in some instances they have been lacking in oxidation resistance, when compared to nickel base alloys. However, at high temperatures, on the order of 1800 to 2100 F. nickel base alloys have limited mechanical properties. Accordingly, it would represent an advance in the art if cobalt base alloys could be provided with oxidation resistance comparable to or better than that of nickel base alloys at high temperatures, while retaining the characteristic strength and mechanical properties of cobalt base alloys at high temperatures.

 

Table 1 : Standard Cobalt cobalt alloy Alloy 

  Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -      
  Hastelloy C22®(UNS N06022)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
  Hastelloy C276®(UNS N10276)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
  Hastelloyx®(UNS N06002)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W other
  0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
  Monel 400®(UNS NO4400) (Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 1  
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63 min 28-34 2.5
  Monel M400®(UNS NO4400)(Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 2
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63-70 28-34 2.5
  Monel R405®(UNS NO4405)(Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 3
  C MN S Si Ni Cu Fe
  0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
  Monel K500®(UNS NO5500)(Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 4  
  C MN S Si Ni Cu Ti AI Fe
  0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
  Inconel 600(UNS NO6600)(Max.)  
  C MN S Si Cr Ni Cu Fe  
  0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
  Inconel 601(UNS NO6601)(Max.)
  C MN Si Cr Ni CO AI Fe
  0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
  Inconel 718(UNS NO7718)(Max.)
  Cr Ni Mo CO Cb+Ta Ti AI Fe
  19 52.5min 3.05 5 5.13 0.9 0.5 18.5
  Chemical Analysis of Incoloy 800® uns(N08800)  
  C Cr Ni Ti AI Fe Grain
  0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
  Incoloy800H® UNS(N08810)
  C Cr Ni Ti AI Fe Grain
  0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
  Incoloy800HT® UNS(N08811)
  C Cr Ni Ti AI Fe Grain
  0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

 

Dimensions:as per drawings

 

 

 

Production Process

Step 1: Getting orders.

 

Step 2: Process design by technical department

 

Step 3: Purchase of raw materials and pattern making &checking

 

Step 4: Inspection of raw materials

 

Step 5: Melting by middle-frequency induction furnaces

 

Step 6: Ladle analysis by Spectrometer

 

Step 7: De-oxidization, slag-removal, tapping

 

Step 8: Pouring

 

Step 9: Openning & fettling

 

Step 10: Surface & dimensional check

 

Step 11: Heat treatment

 

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

 

Step 13: Packing

 

Step 14: Shipping

 

 

cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 5

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

 

 

Our Trade Show cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 6

 

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

 

 

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

www.ebcastings.com

 

Eternal Bliss Alloy Casting & Forging Co.,LTD.

 

Add.: J-Sci-Tech Park, Binhu District,Wuxi,214122, Jiangsu,China

 
products
PRODUCTS DETAILS
cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054
MOQ: 30 kg
Price: USD80/kg ~ USD120/kg
Standard Packaging: Pallets
Delivery Period: It depends on the quantity to be ordered.
Payment Method: by T/T or L/C, Western Union
Supply Capacity: 100,000,000.00
Detail Information
Place of Origin
China
Brand Name
Eternal Bliss
Certification
ISO9001-2008
Model Number
EB26054
Hardness:
More Than HRC 43
Material:
Cobalt Alloy 7
Working Temperature:
Up To 1300 Degree
Corrosion Resistance:
High
Size Tolerance After Casting:
CT7
Certification:
ISO9001
Minimum Order Quantity:
30 kg
Price:
USD80/kg ~ USD120/kg
Packaging Details:
Pallets
Delivery Time:
It depends on the quantity to be ordered.
Payment Terms:
by T/T or L/C, Western Union
Supply Ability:
100,000,000.00
Highlight

precision steel casting

,

cobalt based alloys

Product Description

cobalt alloy 7 Cobalt Castings High Temperature Up to 1300 Degree Wax Cast Process EB26054

cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 0

We produce High Temperature Superalloy Castings Parts with centrifugal cast process, investment process and resin sand cast process.

 

Cobalt base alloys have been used extensively in the past for high temperature applications and have been found to be generally satisfactory except that in some instances they have been lacking in oxidation resistance, when compared to nickel base alloys. However, at high temperatures, on the order of 1800 to 2100 F. nickel base alloys have limited mechanical properties. Accordingly, it would represent an advance in the art if cobalt base alloys could be provided with oxidation resistance comparable to or better than that of nickel base alloys at high temperatures, while retaining the characteristic strength and mechanical properties of cobalt base alloys at high temperatures.

 

Table 1 : Standard Cobalt cobalt alloy Alloy 

  Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -      
  Hastelloy C22®(UNS N06022)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
  Hastelloy C276®(UNS N10276)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
  Hastelloyx®(UNS N06002)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W other
  0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
  Monel 400®(UNS NO4400) (Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 1  
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63 min 28-34 2.5
  Monel M400®(UNS NO4400)(Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 2
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63-70 28-34 2.5
  Monel R405®(UNS NO4405)(Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 3
  C MN S Si Ni Cu Fe
  0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
  Monel K500®(UNS NO5500)(Max.)cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 4  
  C MN S Si Ni Cu Ti AI Fe
  0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
  Inconel 600(UNS NO6600)(Max.)  
  C MN S Si Cr Ni Cu Fe  
  0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
  Inconel 601(UNS NO6601)(Max.)
  C MN Si Cr Ni CO AI Fe
  0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
  Inconel 718(UNS NO7718)(Max.)
  Cr Ni Mo CO Cb+Ta Ti AI Fe
  19 52.5min 3.05 5 5.13 0.9 0.5 18.5
  Chemical Analysis of Incoloy 800® uns(N08800)  
  C Cr Ni Ti AI Fe Grain
  0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
  Incoloy800H® UNS(N08810)
  C Cr Ni Ti AI Fe Grain
  0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
  Incoloy800HT® UNS(N08811)
  C Cr Ni Ti AI Fe Grain
  0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

 

Dimensions:as per drawings

 

 

 

Production Process

Step 1: Getting orders.

 

Step 2: Process design by technical department

 

Step 3: Purchase of raw materials and pattern making &checking

 

Step 4: Inspection of raw materials

 

Step 5: Melting by middle-frequency induction furnaces

 

Step 6: Ladle analysis by Spectrometer

 

Step 7: De-oxidization, slag-removal, tapping

 

Step 8: Pouring

 

Step 9: Openning & fettling

 

Step 10: Surface & dimensional check

 

Step 11: Heat treatment

 

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

 

Step 13: Packing

 

Step 14: Shipping

 

 

cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 5

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

 

 

Our Trade Show cobalt alloy 7 Cobalt Alloy Castings High Temperature 1300 Degree Wax Cast Process EB26054 6

 

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

 

 

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

www.ebcastings.com

 

Eternal Bliss Alloy Casting & Forging Co.,LTD.

 

Add.: J-Sci-Tech Park, Binhu District,Wuxi,214122, Jiangsu,China

 
Sitemap |  Privacy Policy | China Good Quality Nickel Alloy Casting Supplier. Copyright © 2018-2024 Eternal Bliss Alloy Casting & Forging Co.,LTD. . All Rights Reserved.