Products
PRODUCTS DETAILS
Home > Products >
Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

MOQ: 30 kg
Price: USD80/kg ~ USD120/kg
Standard Packaging: Pallets
Delivery Period: It depends on the quantity to be ordered.
Payment Method: by T/T or L/C, Western Union
Supply Capacity: 100,000,000.00
Detail Information
Place of Origin
China
Brand Name
Eternal Bliss
Certification
ISO9001-2008
Model Number
EB26078
Material Grade:
Cobalt Alloy 1, Cobalt Alloy 3,
Hardness Temperature:
Up To 1200 Centi-degree
Coating Process:
SPF Coating,overlay Process
Cast Process:
Wax Lost Process
Surface Treatment:
Shot Blast
Standard:
ASTM B392
Service:
OEM\ODM
Heattreatment:
Solution Annealing And Aging
Type:
Bolts
Quality Control:
100% Inspected
Hardness:
HRC 40 - 60
Grade:
Cobalt Alloy 21
Wearresistance:
High
Usage:
Oil And Gas Industry
Thermalconductivity:
15 - 25 W/m·K
Shape:
Irregular Shape/Spherical Powder
Use:
Ore Mining
Castingmethod:
Investment Casting, Sand Casting
Drawing Made:
Accept
Appearance:
Silvery
Highlight:

precision steel casting

,

cast cobalt alloys

Product Description

Precision Cast Process X-40 Cobalt High Speed Steel Products with High Accuracy EB26078

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products.

 

Precision investment casting services for a variety of high temperature super alloys cobalt-based types.

Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.

 

We produce High Temperature Superalloy Castings Parts with precision investment process.

 

Table 1 : Standard Cobalt cobalt alloy Alloy 

  Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -      
  Hastelloy C22®(UNS N06022)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
  Hastelloy C276®(UNS N10276)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
  Hastelloyx®(UNS N06002)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W other
  0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
  Monel 400®(UNS NO4400) (Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products  
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63 min 28-34 2.5
  Monel M400®(UNS NO4400)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63-70 28-34 2.5
  Monel R405®(UNS NO4405)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  C MN S Si Ni Cu Fe
  0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
  Monel K500®(UNS NO5500)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products  
  C MN S Si Ni Cu Ti AI Fe
  0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
  Inconel 600(UNS NO6600)(Max.)  
  C MN S Si Cr Ni Cu Fe  
  0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
  Inconel 601(UNS NO6601)(Max.)
  C MN Si Cr Ni CO AI Fe
  0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
  Inconel 718(UNS NO7718)(Max.)
  Cr Ni Mo CO Cb+Ta Ti AI Fe
  19 52.5min 3.05 5 5.13 0.9 0.5 18.5
  Chemical Analysis of Incoloy 800® uns(N08800)  
  C Cr Ni Ti AI Fe Grain
  0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
  Incoloy800H® UNS(N08810)
  C Cr Ni Ti AI Fe Grain
  0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
  Incoloy800HT® UNS(N08811)
  C Cr Ni Ti AI Fe Grain
  0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

 

Dimensions:as per drawings

 

 

Production Process

Step 1: Getting orders.

 

Step 2: Process design by technical department

 

Step 3: Purchase of raw materials and pattern making &checking

 

Step 4: Inspection of raw materials

 

Step 5: Melting by middle-frequency induction furnaces

 

Step 6: Ladle analysis by Spectrometer

 

Step 7: De-oxidization, slag-removal, tapping

 

Step 8: Pouring

 

Step 9: Openning & fettling

 

Step 10: Surface & dimensional check

 

Step 11: Heat treatment

 

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

 

Step 13: Packing

 

Step 14: Shipping

 

 

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

 

 

Our Trade Show Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

 

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

 

 

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Productswww.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.
 
 
Products
PRODUCTS DETAILS
Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
MOQ: 30 kg
Price: USD80/kg ~ USD120/kg
Standard Packaging: Pallets
Delivery Period: It depends on the quantity to be ordered.
Payment Method: by T/T or L/C, Western Union
Supply Capacity: 100,000,000.00
Detail Information
Place of Origin
China
Brand Name
Eternal Bliss
Certification
ISO9001-2008
Model Number
EB26078
Material Grade:
Cobalt Alloy 1, Cobalt Alloy 3,
Hardness Temperature:
Up To 1200 Centi-degree
Coating Process:
SPF Coating,overlay Process
Cast Process:
Wax Lost Process
Surface Treatment:
Shot Blast
Standard:
ASTM B392
Service:
OEM\ODM
Heattreatment:
Solution Annealing And Aging
Type:
Bolts
Quality Control:
100% Inspected
Hardness:
HRC 40 - 60
Grade:
Cobalt Alloy 21
Wearresistance:
High
Usage:
Oil And Gas Industry
Thermalconductivity:
15 - 25 W/m·K
Shape:
Irregular Shape/Spherical Powder
Use:
Ore Mining
Castingmethod:
Investment Casting, Sand Casting
Drawing Made:
Accept
Appearance:
Silvery
Minimum Order Quantity:
30 kg
Price:
USD80/kg ~ USD120/kg
Packaging Details:
Pallets
Delivery Time:
It depends on the quantity to be ordered.
Payment Terms:
by T/T or L/C, Western Union
Supply Ability:
100,000,000.00
Highlight

precision steel casting

,

cast cobalt alloys

Product Description

Precision Cast Process X-40 Cobalt High Speed Steel Products with High Accuracy EB26078

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products.

 

Precision investment casting services for a variety of high temperature super alloys cobalt-based types.

Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.

 

We produce High Temperature Superalloy Castings Parts with precision investment process.

 

Table 1 : Standard Cobalt cobalt alloy Alloy 

  Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -      
  Hastelloy C22®(UNS N06022)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
  Hastelloy C276®(UNS N10276)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
  Hastelloyx®(UNS N06002)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W other
  0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
  Monel 400®(UNS NO4400) (Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products  
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63 min 28-34 2.5
  Monel M400®(UNS NO4400)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63-70 28-34 2.5
  Monel R405®(UNS NO4405)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  C MN S Si Ni Cu Fe
  0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
  Monel K500®(UNS NO5500)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products  
  C MN S Si Ni Cu Ti AI Fe
  0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
  Inconel 600(UNS NO6600)(Max.)  
  C MN S Si Cr Ni Cu Fe  
  0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
  Inconel 601(UNS NO6601)(Max.)
  C MN Si Cr Ni CO AI Fe
  0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
  Inconel 718(UNS NO7718)(Max.)
  Cr Ni Mo CO Cb+Ta Ti AI Fe
  19 52.5min 3.05 5 5.13 0.9 0.5 18.5
  Chemical Analysis of Incoloy 800® uns(N08800)  
  C Cr Ni Ti AI Fe Grain
  0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
  Incoloy800H® UNS(N08810)
  C Cr Ni Ti AI Fe Grain
  0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
  Incoloy800HT® UNS(N08811)
  C Cr Ni Ti AI Fe Grain
  0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

 

Dimensions:as per drawings

 

 

Production Process

Step 1: Getting orders.

 

Step 2: Process design by technical department

 

Step 3: Purchase of raw materials and pattern making &checking

 

Step 4: Inspection of raw materials

 

Step 5: Melting by middle-frequency induction furnaces

 

Step 6: Ladle analysis by Spectrometer

 

Step 7: De-oxidization, slag-removal, tapping

 

Step 8: Pouring

 

Step 9: Openning & fettling

 

Step 10: Surface & dimensional check

 

Step 11: Heat treatment

 

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

 

Step 13: Packing

 

Step 14: Shipping

 

 

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

 

 

Our Trade Show Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

 

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

 

 

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Productswww.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.
 
 
sitemap |  Privacy Policy | China Good Quality Nickel Alloy Casting Supplier. Copyright © 2018-2026 Eternal Bliss Alloy Casting & Forging Co.,LTD. . All Rights Reserved.