MOQ: | 30 kg |
Price: | USD80/kg ~ USD120/kg |
Standard Packaging: | Pallets |
Delivery Period: | It depends on the quantity to be ordered. |
Payment Method: | by T/T or L/C, Western Union |
Supply Capacity: | 100,000,000.00 |
Cobalt Alloy Casting Shaft Block and Round Bar for Oil Industry and Valve Ball EB015
1. Product Name: Cobalt Alloy Casting Shaft Block and Round Bar for Oil Industry and Valve Ball EB015
2. Material Grade: Cobalt Alloy
3. Size:OD55x300mm
4. Surface Finish:Ra100
5. Dimensional Tolerance:CT12
6. Application:oil and gas industry
7. Chemical Composition:
Composition (%) | C | Si | Fe | Mo | Ni | Co | Mn | Cr |
Hardness HRC |
≤1.20 | ≤1.20 | ≤3.00 | ≤1.00 | ≤3.00 | ≤Bal | ≤1.00 | ≤29.00 | ≥37 |
8. Cobalt Alloy 6 Physical property (Room Temp.):
Density (lb/in³) |
Specific Gravity | Solidus | Liquidus | Specific heat (J/kg·K) |
Magnetic Permeability |
Electrode Potential |
Electrical Conductivity |
Electrical Resistivity |
0.305 | 8.46 | 2340°F | 2540°F | 0.101°F Btu/lb- |
<1.2@200 Oersteds |
-0.25 Volts |
1.9%IACS (Int.Annealed Copper Std.) |
41.73 microhms-inch |
9. Thermal Properties-Conductivity & Expansion:
Thermal Expansion Coefficient | Thermal Conductivity by Temperature | ||||||
°F | Microinch/ inch-°F |
°C | Microns/ m-°C |
°F | Btu/ft2/in/ hr/°F |
°C | W/mk |
212 | 6.3 | 100 | 11.34 | 70 | 102.7 | 21.11 | 14.82 |
10. Video for Cobalt Alloy Casting Shaft Block and Round Bar for Oil Industry and Valve Ball:
MOQ: | 30 kg |
Price: | USD80/kg ~ USD120/kg |
Standard Packaging: | Pallets |
Delivery Period: | It depends on the quantity to be ordered. |
Payment Method: | by T/T or L/C, Western Union |
Supply Capacity: | 100,000,000.00 |
Cobalt Alloy Casting Shaft Block and Round Bar for Oil Industry and Valve Ball EB015
1. Product Name: Cobalt Alloy Casting Shaft Block and Round Bar for Oil Industry and Valve Ball EB015
2. Material Grade: Cobalt Alloy
3. Size:OD55x300mm
4. Surface Finish:Ra100
5. Dimensional Tolerance:CT12
6. Application:oil and gas industry
7. Chemical Composition:
Composition (%) | C | Si | Fe | Mo | Ni | Co | Mn | Cr |
Hardness HRC |
≤1.20 | ≤1.20 | ≤3.00 | ≤1.00 | ≤3.00 | ≤Bal | ≤1.00 | ≤29.00 | ≥37 |
8. Cobalt Alloy 6 Physical property (Room Temp.):
Density (lb/in³) |
Specific Gravity | Solidus | Liquidus | Specific heat (J/kg·K) |
Magnetic Permeability |
Electrode Potential |
Electrical Conductivity |
Electrical Resistivity |
0.305 | 8.46 | 2340°F | 2540°F | 0.101°F Btu/lb- |
<1.2@200 Oersteds |
-0.25 Volts |
1.9%IACS (Int.Annealed Copper Std.) |
41.73 microhms-inch |
9. Thermal Properties-Conductivity & Expansion:
Thermal Expansion Coefficient | Thermal Conductivity by Temperature | ||||||
°F | Microinch/ inch-°F |
°C | Microns/ m-°C |
°F | Btu/ft2/in/ hr/°F |
°C | W/mk |
212 | 6.3 | 100 | 11.34 | 70 | 102.7 | 21.11 | 14.82 |
10. Video for Cobalt Alloy Casting Shaft Block and Round Bar for Oil Industry and Valve Ball: