Even powder composition, less impurities. High sphericity. Low oxygen content. Good flowability. High loose density, high tap density. 316L stainless steel powder is widely used in powder silver sintering, pressing, metal injection molding, thermal spraying, metal shot blasting and other industries.
| NO. | 304(L) | 316(L) | 17-4PH |
|---|---|---|---|
| Production Process | Atomized | Atomized | Atomized |
| Grade | 304(L) | 316(L) | 17-4PH |
| Density | App.4.1-4.5 Tap.>4.9 G/cm³ | App.4.1-4.5 Tap.>4.8 G/cm³ | App.4.1-4.5 Tap.>4.8 G/cm³ |
| Hardness | 34.5HRC | 36HRC | 35HRC |
| Size | 150um 75um 45um 15um |
150um 75um 45um 15um |
150um 75um 45um 15um |
| Content | Cr:18-20 Ni:8-12 C:0.08(0.03) Si:1max Mn:2max Fe:bal. | Cr:16-18 Ni:10-14 Mo:2-3 C:0.08(0.03) Si:1max Mn:2max Fe:bal. | Cr:15.5-17.5 Ni:3-5 Nb:0.15-0.45 Cu:3-5 C:0.07 Si:1max Mn:1max Fe:bal. |
| Applications | MIM part weight:0.03-200g Apparent relative density>95% Sinter density>7.6g/cm³ sinter temperature:1360-1380°C Shrinkage rate:1.18 | MIM part weight:0.03-200g Apparent relative density>95% Sinter density>7.8g/cm³ sinter temperature:1360-1380°C Shrinkage rate:1.18 | MIM part weight:0.03-200g Apparent relative density>95% Sinter density>7.8g/cm³ sinter temperature:1360-1380°C Shrinkage rate:1.18 |
|
|
| MOQ: | 1 Kilograms |
| Price: | $10.00 - $87.00 / Kilogram |
| Standard Packaging: | Plywood Case: 1500 x 1000 x 1000mm (Max.) 20 feet container: 25 tons (Max.) |
| Delivery Period: | It depends on the quantity to be ordered. |
| Payment Method: | by T/T or L/C,Western Union |
| Supply Capacity: | 100,000.00 |
Even powder composition, less impurities. High sphericity. Low oxygen content. Good flowability. High loose density, high tap density. 316L stainless steel powder is widely used in powder silver sintering, pressing, metal injection molding, thermal spraying, metal shot blasting and other industries.
| NO. | 304(L) | 316(L) | 17-4PH |
|---|---|---|---|
| Production Process | Atomized | Atomized | Atomized |
| Grade | 304(L) | 316(L) | 17-4PH |
| Density | App.4.1-4.5 Tap.>4.9 G/cm³ | App.4.1-4.5 Tap.>4.8 G/cm³ | App.4.1-4.5 Tap.>4.8 G/cm³ |
| Hardness | 34.5HRC | 36HRC | 35HRC |
| Size | 150um 75um 45um 15um |
150um 75um 45um 15um |
150um 75um 45um 15um |
| Content | Cr:18-20 Ni:8-12 C:0.08(0.03) Si:1max Mn:2max Fe:bal. | Cr:16-18 Ni:10-14 Mo:2-3 C:0.08(0.03) Si:1max Mn:2max Fe:bal. | Cr:15.5-17.5 Ni:3-5 Nb:0.15-0.45 Cu:3-5 C:0.07 Si:1max Mn:1max Fe:bal. |
| Applications | MIM part weight:0.03-200g Apparent relative density>95% Sinter density>7.6g/cm³ sinter temperature:1360-1380°C Shrinkage rate:1.18 | MIM part weight:0.03-200g Apparent relative density>95% Sinter density>7.8g/cm³ sinter temperature:1360-1380°C Shrinkage rate:1.18 | MIM part weight:0.03-200g Apparent relative density>95% Sinter density>7.8g/cm³ sinter temperature:1360-1380°C Shrinkage rate:1.18 |